Please wait...
THANKU FOR BEING A PART OF OUR JOURNEY TO BRING "REVOLUTION IN EDUCATION"
We Genuinely APPRECIATE your PATIENCE

44
M: +2.00/-0.66

In orthogonal turning of a cylindrical tube of wall thickness 5 mm, the axial and the tangential cutting forces were measured as 1259 N and 1601 N, respectively. The measured chip thickness after machining was found to be 0.3 mm. The rake angle was 10o and the axial feed was 100 mm/min. the rotational speed of the spindle was 1000 rpm. Assuming the material to be perfectly and Merchant’s first solution, the shear strength of the material is closest to

[GATE ME 2019 Set 1]
A
B
C
D